http://localhost:8080/xmlui/handle/123456789/348| Title: | To evaluate and compare the effect of nanoparticles of titanium dioxide, silicon dioxide and nanocomposite of titanium dioxide – silicon dioxide on tensile strength, tear strength, shore hardness of maxillofacial silicone elastomer: an in-vitro study |
| Authors: | Dr.Sayali Pralhad Hogepatil, IM0218002 |
| Keywords: | Maxillofacial silicone elastomer, SiO2 nanoparticles, TiO2 nanoparticles, TiO2/SiO2 nanocomposite, mechanical properties |
| Issue Date: | 2021 |
| Publisher: | K.L.E. Academy of Higher Education & Research, Belagavi |
| Abstract: | Maxillofacial silicone prosthesis when fabricated present with problems within a few months of their use. These problems are related to the properties concerning the mechanics and physicality of the material. This has been the reason for the researches being circling around the development of this material. PURPOSE The purpose of this study was to evaluate and compare the effect of addition of Titanium Dioxide nanoparticles, Silica Dioxide nanoparticles and Nanocomposite (TiO2/SiO2) on the tensile strength, tear strength and shore hardness of maxillofacial silicone. |
| URI: | http://localhost:8080/xmlui/handle/123456789/348 |
| Appears in Collections: | Prosthodontics |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| IM0218002 Dr.Sayali Pralhad Hogepatil.pdf | 1.38 MB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.